Carbonate stress corrosion cracking is the term applied to surface breaking or cracks that occur adjacent to carbon steel welds under the combined action of ____________ and ___________ in carbonate containing systems.
Carbonate stress corrosion cracking is the term applied to surface breaking or cracks that occur adjacent to carbon steel welds under the combined action of ____________ and ___________ in carbonate containing systems.
A . Temperature, stress
B . Tensile stress, corrosion
C . Corrosion, velocity
D . Tensile stress, velocity
Answer: B