Amine stress corrosion cracking is most often associated with lean amine services. The pure alkanolamine does not cause cracking. Cracking in rich amine services are most often associated with _______ problems.

Amine stress corrosion cracking is most often associated with lean amine services. The pure alkanolamine does not cause cracking. Cracking in rich amine services are most often associated with _______ problems.
A . H²S
B . Stress
C . Wet H²S
D . Temperature

Answer: C